For anodic/ cathodic electro cleaning of copper , brass , zinc and othercopper alloys; contains special
inhibiting / chealting agents to prevent attack on base metal.

Activates treated surface & hence, adhesion to subsequent plating becomes perfect.

 

Operating condition

  • Conc.    50 – 70 g/l
  • Temp.   60 – 80 0C
  • Time     2 - 5 minutes
  • volts      6 to 8 volt