CUPROBRITE 556
Contains organic inhibitor to provide tarnish resistance for copper, copper alloys and copper plated articles
Operating Condition :
- Conc. 10 – 20 ML/l
- Temp. 50 – 60 0C
- Time 1-2 minutes
Contains organic inhibitor to provide tarnish resistance for copper, copper alloys and copper plated articles